黄陵煤显微组分性质及原位热解实验研究

The characteristics of maceral in Huangling coal and its in-situ pyrolysis

  • 摘要: 为了揭示煤中不同组分的热解特征和成焦规律,利用离心分离获取黄陵煤的显微组分富集物,研究显微组分的热解特性,利用显微镜热台原位观测热解过程中显微组分的软化熔融特征。结果发现,镜质组和惰质组富集物的纯度分别可达90%和80%以上,壳质组富集物的纯度接近70%。壳质组的初始热解温度在385 ℃左右,其他显微组分的初始热解温度在410 ℃左右,最大热解温度为470−480 ℃,最大失重速率和热解总失重率均以壳质组、镜质组、半镜质组和惰质组的次序降低。显微热台原位热解实验表明,壳质组(含腐泥基质)的软化温度为350−370 ℃;镜质组的软化温度为410−420 ℃,热解过程经历边缘钝化、气孔产生、表面软化、液相生成和冷却固化等阶段;半镜质组仅呈现微小的形态变化,惰质组未发生变化。黄陵煤中的活性组分为镜质组和壳质组,壳质组对共生镜质组的软化具有促进作用。

     

    Abstract: In order to reveal the pyrolysis and coking characteristics of different components in coal, the macerals in Huangling coal were enriched by centrifugation, and the pyrolysis characteristics of macerals were studied. The transformation characteristics of macerals during pyrolysis were observed in-situ by heating stage microscope. The purities of vitrinite and inertinite are more than 90% and 80%, respectively, while the purity of liptinite is nearly 70%. The initial pyrolysis temperature of liptinite is about 385 ℃, and those of the other macerals are all about 410 ℃. The maximum pyrolysis temperatures are between 470−480 ℃ for all macerals studied. The maximum weight loss rate and the total weight loss rate decrease in the order of liptinite, vitrinite, semi-vitrinite and inertinite. The softening temperature of the liptinite (including sapropelic groundmass) is 350−370 ℃, while that of vitrinite is about 410−420 ℃ as shown by the in-situ pyrolysis in a heating stage microscope. The pyrolysis process of vitrinite goes through the stages of edge shrinking, pore formation, surface softening, the formation of liquid phase, and solidification. Only slight morphological changes are observed in semi-vitrinite, while no changes are observed in inertinite. The active components in Huangling coal are vitrinite and liptinite, and the liptinite can promote the softening and melting characteristics of the adjacent vitrinite.

     

/

返回文章
返回