  • 摘要: 用钌离子催化氧化法探究了晋城15号无烟煤(J15A)的结构特征,结果表明,J15A富含紧密的芳香性结构.在温和条件下,先用H2O2对J15A进行预处理,然后用NaOCl对其氧化从而生成苯多酸.结果表明,H2O2预处理可提高NaOCl氧化J15A生成苯多酸的产率,而且该方法可以高收率、高选择性地获取苯多酸化学品.

     

    Abstract: Jincheng No.15 anthracite (J15A) was subjected to ruthenium ion-catalyzed oxidation to characterize its structural feature. The results show that J15A is abundant in peri-condensed aromatic structure. The NaOCl oxidation of J15A promoted by pretreatment with H2O2 was conducted under mild conditions to produce benzene polycarboxylic acids (BPCAs). The pretreatment with H2O2 is proved to enhance the yields of BPCAs. It is potential to obtain BPCAs in high yield and selectivity by NaOCl oxidation of pretreated J15A with H2O2.

     

/